PotteryCrafts Frit P2963

Alternate Names: Potterycrafts Frit 2963

Description: Soft alkaline very high expansion frit

Oxide Analysis Formula Tolerance
Al2O3 4.90% 0.10
K2O 0.30% 0.01
CaO 26.50% 0.99
MgO 0.10% 0.01
B2O3 10.80% 0.32
SiO2 52.70% 1.83
LOI 4.70%n/a
Oxide Weight 199.36
Formula Weight 209.19

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 14.5
Frit Melting Range (C) 850-1000C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy