PotteryCrafts Frit P2961

Alternate Names: PotteryCrafts Frit 2961

Description: Standard alkaline frit

Oxide Analysis Formula Tolerance
CaO 0.20% 0.02
MgO 0.10% 0.01
K2O 3.40% 0.15
Na2O 12.10% 0.82
Al2O3 7.30% 0.30
B2O3 25.20% 1.53
SiO2 50.40% 3.53
LOI 1.30%n/a
Oxide Weight 415.93
Formula Weight 421.41

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 6.9
Frit Melting Range (C) 900-1100C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy