1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

PotteryCrafts Frit P2960

Alternate Names: PotteryCrafts Frit 2960

Description: Low Expansion Frit

Oxide Analysis Formula Tolerance
CaO 3.70% 0.33
K2O 0.20% 0.01
Li2O 1.10% 0.19
MgO 2.20% 0.27
ZnO 3.20% 0.20
B2O3 17.60% 1.27
Al2O3 8.50% 0.42
SiO2 63.40% 5.30
Oxide Weight 502.28
Formula Weight 502.28

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 3.8
Frit Melting Range (C) 1020-1150C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy