PotteryCrafts Frit P2955

Alternate Names: PotteryCrafts Frit 2955

Description: High alkali low alumina borax frit

Oxide Analysis Formula Tolerance
CaO 8.80% 0.37
K2O 8.80% 0.22
Na2O 10.90% 0.41
B2O3 13.50% 0.46
Al2O3 9.10% 0.21
SiO2 48.90% 1.91
Oxide Weight 234.69
Formula Weight 234.69

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Frit J
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 10.9
Frit Melting Range (C) 920-1050C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy