1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Potclays Frit 2266

Alternate Names: Potclays Ferro Crystal Frit

Description: This is actually Ferro Frit 3110

Oxide Analysis Formula Tolerance
CaO 6.30% 0.29
K2O 2.30% 0.06
Na2O 15.30% 0.64
B2O3 2.60% 0.10
Al2O3 3.70% 0.09
SiO2 69.80% 3.03
Oxide Weight 260.76
Formula Weight 260.76

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy