Potclays Frit 2263

Alternate Names: 2263 Standard boraksfritte, Potclays Standard Borax Frit

Description: High calcium borosilicate frit

Oxide Analysis Formula Tolerance
CaO 15.22% 0.63
K2O 1.33% 0.03
MgO 0.05% -
Na2O 8.75% 0.33
B2O3 18.76% 0.63
Al2O3 7.55% 0.17
SiO2 48.34% 1.88
Oxide Weight 233.76
Formula Weight 233.76

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit CC-250
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy