1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Potash-Silica Eutectic 2

Oxide Analysis Formula Tolerance
K2O 17.50% 1.00
SiO2 82.50% 7.39
Oxide Weight 538.29
Formula Weight 538.29

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 880C