Potash-Alumina-Silica Eutectic

Oxide Analysis Formula Tolerance
K2O 17.30% 1.00
SiO2 77.50% 7.02
Al2O3 5.20% 0.28
Oxide Weight 544.51
Formula Weight 544.51

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 870C