1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Podmore Frit P2250

Description: High alkali frit

Oxide Analysis Formula Tolerance
CaO 6.31% 0.20
K2O 15.90% 0.30
SiO2 50.71% 1.50
Na2O 17.44% 0.50
Al2O3 5.74% 0.10
B2O3 3.91% 0.10
Oxide Weight 177.78
Formula Weight 177.78

Notes

Made by Podmore and Sons
Formerly Frit T

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Potclays Frit 2275
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy