Pleyber G

Oxide Analysis Formula Tolerance
CaO 0.04% -
K2O 1.60% 0.05
MgO 0.22% 0.01
Na2O 0.06% -
TiO2 0.30% 0.01
Al2O3 37.50% 1.00
SiO2 47.50% 2.15
Fe2O3 0.65% 0.01
LOI 12.30%n/a
Oxide Weight 239.01
Formula Weight 272.53

Notes

Particle Size Distribution:
>53 microns: 0.1 max
>10 microns: 8
<2 microns: 61

Modulus of Rupture, Kgf/cm2:
At 80% Relative Humidity: 10.0
Dried at 110C: 21.0

Casting Rate @ 65% solids (mm2/min): 0.35
% P84 Deflocculant Required for 5 Poise Slip: 0.4

1180C 1280C
Fired Absorption: 20% 11%
Fired Shrinkage: 7% 11.5%
Brightness: 90 88

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy