Pioneer Feldspar

Oxide Analysis Formula Tolerance
SiO2 65.40% 6.28 0.35
Al2O3 18.70% 1.06 0.15
K2O 12.00% 0.73 0.4
Na2O 2.85% 0.27 .35
Fe2O3 0.04% - 0.01
LOI 0.35%n/a
Oxide Weight 571.02
Formula Weight 573.03

Notes

Mined in Western Australia at the Sinclair Mine.