Peptapon

Description: Gum, similar to CMC Gum

Notes

Peptapon is an organic gum and binder that can be used almost the same way as CMC. Various grades are available. Its gel isn't transparent like CMC gel - it is thicker using the same amount of water. It is also said to impart hardness without prolonging drying time as much as CMC gum.

Prepare as usual CMC preparation up to 45 gram in 1 liter of very hot water. Mix well using a mechanical mixer if possible, leave for a day and mix again.

Peptapon is especially valuable in high-frit glazes, preventing powdering. It improves the bond between dry glaze and the ware. While it is said to also be a "non-foaming suspension stabilizer", it is not clear exactly what that means. While Peptapon is said to be a suspender, people use a combination of it and bentonite to get better suspending action.

It is produced by the ceramic additives department of ZSCHIMMER & SCHWARZ. This material is used in industry so minimum order quantities put it out of reach of potters or even pottery suppliers.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials CMC Gum
CMC gum is indispensable for many types of ceramic glazes. It is a glue and is mainly used to slow drying and improve adhesion and dry hardness.
Materials Optapix
Troubles Powdering, Cracking and Settling Glazes
Powdering and dusting glazes are difficult and a dust hazard. Shrinking and cracking glazes fall off and crawl. The cause is the wrong amount or type of clay.
Typecodes Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.
URLs http://www.zschimmer-schwarz.com/PEPTAPON_5/simon/zschimmer-schwarz/media/site/downloads/merkblatt/1_K_K_EN_2801_00_1_500.pdf
Peptapon 5 information
Articles Using Dextrin, Glycerine and CMC Gum together

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy