Pemco Frit Pb-906

Alternate Names: Frit Pb906

Description: All-fritted opaque glaze

Oxide Analysis Formula Tolerance
CaO 9.57% 0.58
K2O 2.48% 0.09
Na2O 1.65% 0.09
PbO 15.73% 0.24
Al2O3 5.70% 0.19
B2O3 7.36% 0.36
SiO2 49.49% 2.80
ZrO2 8.00% 0.22
Oxide Weight 340.06
Formula Weight 340.06

Notes

This is Pb-349 wth 8% zirconium silicate. Good base for white and colored opaque glazes. Fires cone 02-6 with 10% clay addition.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit FL-55
Materials Hommel Frit 2GF6K
Materials Ferro Frit 3565
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.20
Co-efficient of Linear Expansion 6.2 x 10-6 (40-450C)
Frit Softening Point 1550F
Frit Melting Range (C) 1500-1670F
I.F.P. (celsius) 675C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy