1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit Pb-461

Alternate Names: Frit Pb461

Description: Very low expansion lead-borosilicate

Oxide Analysis Formula Tolerance
PbO 43.20% 1.00
B2O3 21.90% 1.63
SiO2 34.90% 3.00
Oxide Weight 516.67
Formula Weight 516.67

Notes

Added to glazes to prevent crazing, also used in low fire cone 012-06 glazes.

Related Information

Links

Materials Pemco Frit P-941
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-8
Materials Hommel Frit 1006
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.20
Co-efficient of Linear Expansion 5.2 x 10-6 (50-450C)
Frit Softening Point 1480F
Frit Melting Range (C) 1460-1500F
I.F.P. (celsius) 525C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy