Pemco Frit P-941

Alternate Names: Frit 941, Frit P941

Description: Magnesia-alumina-silica eutectic

Oxide Analysis Formula Tolerance
CaO 3.30% 0.13
MgO 16.10% 0.87
Al2O3 19.60% 0.42
SiO2 61.00% 2.21
Oxide Weight 218.18
Formula Weight 218.18

Notes

Has very low expansion but is much higher melting that Pb-461. Use this to improve craze resistance.

Related Information

Links

Materials Pemco Frit Pb-461
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 4.4 x 10-6 (50-450C)
Frit Melting Range (C) 2250-2320F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy