1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit Pb-1R99

Alternate Names: Frit Pb1R99

Description: High expansion lead flux for cone 06 glazes

Oxide Analysis Formula Tolerance
K2O 4.40% 0.13
Na2O 10.90% 0.47
PbO 33.30% 0.40
B2O3 12.00% 0.46
Al2O3 7.40% 0.20
SiO2 31.90% 1.43
Oxide Weight 268.76
Formula Weight 268.76

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 12.60
Co-efficient of Linear Expansion 12.6 x 10-6 (50-350C)
Frit Softening Point 1170F
Frit Melting Range (C) 1150-1200F
I.F.P. (celsius) 425C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy