Pemco Frit P-760

Alternate Names: Frit 760, Frit P760

Description: Cadmium bearing frit

Oxide Analysis Formula Tolerance
CdO 7.40% 0.22
K2O 8.10% 0.33
Na2O 7.30% 0.45
B2O3 16.30% 0.90
Al2O3 4.30% 0.16
SiO2 56.60% 3.60
Oxide Weight 382.62
Formula Weight 382.62

Notes

Used in all-fritted glazes with Pb-41 as base for low temperature cadmium-selenium type colors.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.90
Frit Melting Range (C) 1330-1440F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy