Pemco Frit P-609

Alternate Names: Frit 609, Frit P609

Description: LEADLESS FRIT

Oxide Analysis Formula Tolerance
CaO 7.10% 0.32
K2O 1.10% 0.03
Li2O 1.70% 0.14
MgO 3.30% 0.21
Na2O 2.20% 0.09
SrO 8.50% 0.21
B2O3 9.00% 0.33
Al2O3 8.00% 0.20
SiO2 59.10% 2.49
Oxide Weight 253.36
Formula Weight 253.36

Notes

Component for partially-fritted leadless glazes firing cone 4-8.

Related Information

Links

Materials Fusion Frit F-76
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 3GF84C
Materials Fusion Frit F-524
A low fire base glaze, add 10% kaolin, adjust thermal expansion using other frits.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.9 x 10-6 (50-450C)
Frit Melting Range (C) 1430-1530F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy