1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit P-2G63

Alternate Names: 2G63,2G-63

Description: Highly opaque frit for use in all-fritted cone 06-6 glazes

Oxide Analysis Formula Tolerance
CaO 1.50% 0.17
MgO 0.20% 0.03
Na2O 7.60% 0.78
ZnO 0.20% 0.02
ZrO2 11.30% 0.59
B2O3 17.10% 1.57
Al2O3 5.50% 0.34
SiO2 56.60% 6.01
Oxide Weight 638.01
Formula Weight 638.01

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit FZ-284
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.50
Co-efficient of Linear Expansion 6.50 (50-450C)
Frit Softening Point 1550F
Frit Melting Range (C) 1520-1620F
Co-efficient of Linear Expansion 6.5x10-6 (50-450C)
I.F.P. (celsius) 569C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy