Fusion Frit FZ-284

Alternate Names: Frit FZ284

Description: Zircon frit

Oxide Analysis Formula Tolerance
CaO 1.70% 0.20
Na2O 7.60% 0.79
ZnO 0.20% 0.02
ZrO2 11.30% 0.59
B2O3 17.10% 1.58
Al2O3 5.50% 0.35
SiO2 56.60% 6.06
Oxide Weight 643.75
Formula Weight 643.75

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-2G63
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy