Pemco Frit P-1R63

Alternate Names: 1R-63,1R63

Oxide Analysis Formula Tolerance
CaO 14.30% 0.67
K2O 0.40% 0.01
Na2O 7.50% 0.32
ZrO2 9.60% 0.20
B2O3 16.60% 0.63
Al2O3 4.40% 0.11
SiO2 46.70% 2.04
Oxide Weight 261.76
Formula Weight 261.76

Notes

Similar to P-926 containing 10% zirconia

Related Information

Links

Materials Pemco Frit P-926
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-49
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.80
Co-efficient of Linear Expansion 7.80 (50-450C)
Frit Softening Point 1550F
Frit Melting Range (C) 1500-1600F
Co-efficient of Linear Expansion 7.8x10-6 (50-450C)
I.F.P. (celsius) 662C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy