Palygorskite

Oxide Analysis Formula Tolerance
CaO 1.20% 0.07
MgO 10.30% 0.87
K2O 1.20% 0.04
Na2O 0.20% 0.01
Al2O3 13.20% 0.44
SiO2 69.50% 3.95
Fe2O3 4.50% 0.10
Oxide Weight 341.71
Formula Weight 341.71

Notes

The same as attapulgite, this is just another sample analysis.

Related Information

Links

Materials Attapulgite
Materials Sepiolite
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.
Minerals Attapulgite, Palygorskite
Attapulgite is a magnesium aluminum silicate clay of very fine particle size. It is also known as Fu

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy