1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Oxford Feldspar

Description: Potash Feldspar

Oxide Analysis Formula Tolerance
CaO 0.39% 0.05
K2O 8.07% 0.59
Na2O 3.28% 0.36
Al2O3 17.35% 1.17
SiO2 70.82% 8.10
Fe2O3 0.09% -
LOI 0.18%n/a
Oxide Weight 687.17
Formula Weight 688.41

Notes

This material is no longer available. In determining a substutite considering the proportion of K2O to Na2O in the formula is helpful.
Eureka #703, Kona A-3 or Custer feldspar are a good substitutes.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy