Opeal OP-1 Ball Clay

Description: Super-white ball clay

Oxide Analysis Formula Tolerance
SiO2 60.47% 3.60
Al2O3 28.52% 1.00
Fe2O3 0.28% 0.01
TiO2 0.33% 0.01
CaO 0.02% -
MgO 0.03% -
K2O 0.45% 0.02
Na2O 0.10% 0.01
LOI 9.80%n/a
Oxide Weight 322.59
Formula Weight 357.64

Notes

Developed according to current popular Super-white polished tiles and high-grade tableware. This product has a outstanding whiteness after burning(whiteness above 90 degree after 1220℃ burning) and it shows the best level in refined ball clay field.

Related Information

Links

URLs http://www.opeal.com.cn/english/products_op01.htm
Opeal OP-1 Ball clay information
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy