Novacite Silica 1

Alternate Names: Whetstone

Description: Microcrystalline Novaculite

Oxide Analysis Formula Tolerance
CaO 0.01% 0.18
MgO 0.02% 0.51
TiO2 0.01% 0.13
Al2O3 0.10% 1.00
SiO2 99.49%
Fe2O3 0.04% 0.26
Oxide Weight 101,663.40
Formula Weight 101,663.40

Notes

Novacite® is a quartz silica unique in the extender/filler market. Graded by micron size, the individual, unagglomerated particles tend toward a platey structure, which promotes superior leveling, meshing and wear-resistance in many performance applications.

Mined and processed in Hot Springs, Arkansas, USA. The product is a "rotted", or powdered form of Novaculite mineral. It is also known as Arkansas Whetstone because it is a massive white quartz rock used to make whetstones for sharpening knives.

According to the Arkansas Geological Commission it is "a sedimentary rock composed mostly of microcrystalline quartz and is a recrystallized variety of chert. It is dense, hard, white to grayish-black in color, translucent on thin edges, and has a dull to waxy luster.".

Typical applications other than ceramics include casting resins, potting compounds, molding compounds, abrasive medium (wet blasting), latex paints.

Color (Dry): White
Color (Wet): Grey
Particle Shape (1-7 microns): Platey (over 7 microns): Clusters
Specific Heat (mean 0-200C): 192 cal/g/degree C
Surface Modification: Very Receptive

Related Information


This picture has its own page with more detail, click here to see it.

Emeralds Mix

Links

URLs http://www.state.ar.us/agc/novaculi.htm
Arkansas Geological Commission
URLs http://www.fs.fed.us/oonf/history/nova/novaculite.htm
Geology information
URLs http://www.fs.fed.us/oonf/history/quarry_pic.html
Quarry pictures
URLs http://www.thomasregister.com/olc/malvernminerals/page2.htm
Malvern Minerals Product page
URLs http://www.thomasregister.com/olc/malvernminerals/page2.htm
Malvern Minerals Product Page
Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.

Data

Density, loose packed (lbs/cu fut) 50 lbs/cubic foot
Hardness (Moh) 7
Index of Refraction 1.55
Oil Adsorption (Spatula) 17-20%
Particle Shape (1-7 microns) Platey (over 7 microns): Clusters
Sieve Analysis Dry Percent finer that 74 microns: 99 53 microns: 98 44 microns: 93-98 10 microns: 36 Average parti
Density (Specific Gravity) 2.65
pH for dry powder 6.0-7.8

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy