Neodymium Oxide

Alternate Names: Lanthanide

Oxide Analysis Formula Tolerance
Nd2O3 100.00% 1.00
Oxide Weight 336.48
Formula Weight 336.48

Notes

This is a lanthanide rare earth oxide, it is available as a raw pale blue/lavender powder.
It is used as a colorant and acts as a flux.

For information on making vibrant colors using lanthanides visit the page by David Pier linked to this record.

Quote from David Pier: "The oxide is a blue/lavender powder. It is the strongest of these three colorants, giving a good aqua color in most glaze bases at 1-2%. At 4-7% it gives a pleasant lavender/grape color that appears as a different color under different artificial light sources. It is very strongly affected by iron, particularly in oxidation, giving a reliable perfect neutral transparent gray. Avoid trace iron impurities to achieve the brightest blue and lavender colors."

Related Information

Links

URLs http://www.lagunaclay.com/news/rare.htm
New glaze colors using lanthanides
URLs http://www.americanelements.com/nd.html
American Elements, a supplier
Temperatures Neodymium oxide melts (2320-)
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy