1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Natron Feldspar

Description: Soda feldspar

Oxide Analysis Formula Tolerance
Na2O 7.50% 0.65
Al2O3 19.10% 1.00
K2O 2.80% 0.16
CaO 2.00% 0.19
SiO2 68.40% 6.11
Fe2O3 0.10% -
Oxide Weight 536.11
Formula Weight 536.11

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.