Oxide Analysis Formula Tolerance
K2O 28.70% 0.45
Na2O 23.50% 0.55
B2O3 47.80% 1.00
Oxide Weight 146.26
Formula Weight 146.26

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 855C