Mullite Fused Zircon

Oxide Analysis Formula Tolerance
CaO 0.10% -
K2O 0.10% -
MgO 0.10% 0.01
Na2O 0.10% -
TiO2 0.10% -
Al2O3 45.50% 1.00
36.90% -
SiO2 17.30% 0.65
Oxide Weight 141.90
Formula Weight 141.90

Notes

Particle Size: 0.7-1.5mm
Free iron grains: .02% max
Grain porosity: 1.5%
Bulk density: 3.65 g/cm3
Refractoriness: 1743C

Related Information

Links

Typecodes Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes.

Data

Density (Specific Gravity) 3.67