Oxide Analysis Formula Tolerance
Na2O 15.61% 1.00
Al2O3 5.14% 0.20
B2O3 26.29% 1.50
SiO2 52.96% 3.50
Oxide Weight 397.18
Formula Weight 397.18

Notes

Corrected chemistry of this frit Oct 2022, it was:
BaO 26.3, Na2O 15.6, Al2O3 5.1, SiO2 53.0

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 565C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy