Moulin Fritte M74

Description: Ancienne fritte

Oxide Analysis Formula Tolerance
CaO 9.84% 0.45
K2O 3.67% 0.10
PbO 39.15% 0.45
B2O3 12.21% 0.45
SiO2 35.14% 1.50
Oxide Weight 256.59
Formula Weight 256.59

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.