Oxide Analysis Formula Tolerance
BaO 39.75% 1.00
Al2O3 13.49% 0.51
SiO2 46.76% 3.00
Oxide Weight 385.66
Formula Weight 385.66

Notes

Corrected this wrong analysis Oct 2022:
BaO 47.0, Al2O3 16.0, SiO2 37.0

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 855C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy