Minspar 1

Description: Coarse grained glass feldspar

Oxide Analysis Formula Tolerance
CaO 1.50% 0.15
K2O 4.10% 0.25
Na2O 6.50% 0.60
Al2O3 18.50% 1.04
SiO2 68.60% 6.52
Fe2O3 0.06% -
LOI 0.30%n/a
Oxide Weight 566.87
Formula Weight 568.58

Notes

Spruce Pine, NC
A minus 30 mesh feldspar product used in the glass container and ceramic tile markets.

Physical Properties
===================
Specific Gravity: 2.6
Refractive Index: 1.53
Mohs Hardness: 6-6.5
Mean Particle Size, microns: n/a
Specific Surface Area, sq metre/g: n/a
Dry Brightness (Green Filter): n/a
Raw color: white
pH: n/a
% Moisture Content: 0.1
Bulk Density (lb/cu. ft)
Loose: 95.0
Packed: 100

Structure: Crystalline
Particle Shape: Granular

Particle Size: 16 20 30 40 100 140 170 200 325
% Retained 0.0 0.0 0.7 11.3 60.0 12.0 10.0
U.S. Sieve Series

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy