Oxide Analysis Formula Tolerance
CaO 21.51% 0.30
K2O 33.44% 0.28
MgO 15.85% 0.31
Na2O 2.30% 0.03
P2O5 16.34% 0.09
SiO2 0.67% 0.01
Fe2O3 0.58% -
MnO 2.60% 0.03
SO3 6.71%n/a
Oxide Weight 72.66