MC Blend

Oxide Analysis Formula Tolerance
K2O 1.10% 0.04
Na2O 0.20% 0.01
MgO 0.40% 0.03
CaO 0.20% 0.01
TiO2 1.80% 0.08
Fe2O3 0.90% 0.02
Al2O3 29.00% 1.00
SiO2 55.60% 3.25
LOI 11.40%n/a
Oxide Weight 313.74
Formula Weight 354.11

Notes

If you know more about this material please contact us.

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

Data

Pyrometric Cone Equivalent 32