Masterfil Kaolin

Oxide Analysis Formula Tolerance
CaO 0.10% -
K2O 0.22% 0.01
MgO 0.05% -
Na2O 0.02% -
TiO2 1.78% 0.06
Al2O3 37.78% 1.00
SiO2 45.92% 2.06
Fe2O3 0.69% 0.01
LOI 13.11%n/a
Oxide Weight 233.70
Formula Weight 268.96

Notes

A general purpose air floated kaolin of good casting properties. It is an appropriate selection for mechanical forming applications where more plasticity is desirable and fired color is not critical.

Bulk Density: 30 lb/cu. ft.
Moisture: 1%
PCE: 34
C.E.C.: 3.5
Specific Gravity: 2.62
pH (10% solids, max.): 6.0
Viscosity (70% solids, cps): 1000
Wet Sieve Residue, +325 mesh (%): 1.0
Median Particle Diameter (microns): 1.2
Specific Surface Area (sq. meters/gram): 17.31

Particle Size (% finer than):
20 microns: 93.6
10: 84.3
5: 73.1
2: 57.8
1: 46.8
0.5: 32.9

Related Information

Links

URLs http://www.zemex.com/feldspar/master.html
Zemex Feldspar Data Sheets
Materials Mastercast Kaolin
Materials Masterfloat Kaolin
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy