Madoc Feldspar

Alternate Names: Madoc Spar, Madoc H Feldspar

Description: Legacy Potash feldspar

Oxide Analysis Formula Tolerance
K2O 8.89% 0.62
Na2O 3.59% 0.38
Al2O3 17.39% 1.12
SiO2 68.63% 7.50
Oxide Weight 646.85
Formula Weight 646.85

Notes

Another formula for Madoc:
K2O 0.61
Na2O 0.34
CaO 0.05
Al2O3 1.04
SiO2 6.4

Related Information

Links

Materials Potash Feldspar
A feldspar having a KNaO content that predominates in potassium.
Materials Soda Feldspar
A feldspar having a KNaO content that predominates in sodium.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy