M&M Ball Clay

Description: Legacy ball clay from Moore and Munger

Oxide Analysis Formula Tolerance
SiO2 47.90% 2.56
Al2O3 31.70% 1.00
Fe2O3 1.00% 0.02
TiO2 1.00% 0.04
CaO 0.20% 0.01
MgO 0.50% 0.04
K2O 0.50% 0.02
Na2O 2.40% 0.12
LOI 14.60%n/a
Oxide Weight 274.15
Formula Weight 321.01

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

Data

Drying Shrinkage 5.0%
Firing Shrinkage 13% at cone 9
Dry M.O.R. (50% Silica) 510 psi