Lithospar

Oxide Analysis Formula Tolerance
K2O 2.91% 0.19
Li2O 2.00% 0.41
Na2O 4.04% 0.40
Al2O3 21.69% 1.30
SiO2 69.36% 7.07
Oxide Weight 612.87
Formula Weight 612.87

Notes

Has lower lithium than petalite, spodumene and lepidolite.
While the term lithium feldspar is commonly used in the ceramic industry, there is no such thing (for example, in references that list various types of feldspar, no lithium material appears). The lithium ion is too small to be a part of the feldspar crystal structure.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy