Klondike Kaolin

Description: Legacy white kaolin from Edgar Bros. Co.

Oxide Analysis Formula Tolerance
SiO2 42.01% 1.72
Al2O3 41.48% 1.00
Fe2O3 0.30% -
TiO2 0.70% 0.02
CaO 0.60% 0.03
MgO 0.50% 0.03
K2O 0.50% 0.01
Na2O 0.50% 0.02
LOI 13.60%n/a
Oxide Weight 212.93
Formula Weight 246.44

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

% < 0.5 microns 17%
Drying Shrinkage 3%
Dry M.O.R. (50% Silica) 65

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy