1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Kaolin 233

Oxide Analysis Formula Tolerance
SiO2 49.30% 2.36
Al2O3 35.50% 1.00
Fe2O3 0.39% 0.01
TiO2 0.39% 0.01
K2O 1.74% 0.05
Na2O 0.14% 0.01
CaO 0.02% -
MgO 0.10% 0.01
P2O5 0.19% -
H2O 12.10%n/a
Oxide Weight 252.18
Formula Weight 286.90

Notes

85% kaolinite, 10% K Spar, 1% N Spar, 2% Quartz

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
Minerals Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How
Minerals K-Feldspar
Most common feldspars contain both sodium and potassium. The term K-Feldspar designates one where th
Minerals Na-Feldspar
Most common feldspars contain both sodium and potassium. The term Na-Feldspar designates one where t
Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy