Kamonkoli Ball Clay

Description: Uganda ball clay

Oxide Analysis Formula Tolerance
MgO 0.23% 0.02
Al2O3 23.42% 1.00
Na2O 0.13% 0.01
SiO2 54.78% 3.97
P2O5 0.14% -
K2O 1.02% 0.05
CaO 0.46% 0.04
TiO2 1.83% 0.10
Fe2O3 7.33% 0.20
Cr2O3 0.02% -
MnO 0.03% -
CuO 0.02% -
ZrO2 0.10% -
LOI 10.02%n/a
SO3 0.29%n/a
Oxide Weight 389.84
Formula Weight 434.65

Notes

Analysis from SEAMIC labs in 2007.

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy