1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

K Metaborate and KBO2.KPO3 Eutectic

Oxide Analysis Formula Tolerance
K2O 45.70% 0.77
P2O5 20.40% 0.23
B2O3 33.90% 0.77
Oxide Weight 159.01
Formula Weight 159.01

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 770C

PayPal