Description: Zinc barium calcium alkali frit (formerly #FT0540)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 3.00% | 0.06 | |
| CaO | 11.00% | 0.58 | |
| KNaO | 9.00% | 0.34 | |
| ZnO | 10.00% | 0.36 | |
| B2O3 | 6.00% | 0.25 | |
| Al2O3 | 8.00% | 0.23 | |
| SiO2 | 56.00% | 2.75 | |
| Oxide Weight | 304.29 | ||
| Formula Weight | 304.29 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 0.335 @ 500C |
|---|