March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | Feb 14-15, 2026 - Major Server Upgrade Done | No tracking! No ads! |
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.02% | - | |
| K2O | 3.20% | 0.14 | |
| MgO | 0.47% | 0.05 | |
| Al2O3 | 25.20% | 1.00 | |
| SiO2 | 61.20% | 4.12 | |
| Fe2O3 | 1.74% | 0.04 | |
| TiO2 | 1.04% | 0.05 | |
| Na2O | 0.16% | 0.01 | |
| LOI | 11.00% | n/a | |
| Oxide Weight | 376.55 | ||
| Formula Weight | 423.09 | ||
Manufacturer says: A nice white clay in the raw state. Fires to a cream color.
Physical data can be found on the link to the product information web page of the manufacturer.
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| URLs |
https://www.clayimco.com/industrial-clays
IMCO information on their mined clays |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk