Ibex Bentonite

Alternate Names: Ibex-200 Bentonite, Ibex 200 Bentonite

Description: Calcium Low-swell Bentonite

Oxide Analysis Formula Tolerance
CaO 10.80% 0.34
K2O 3.50% 0.07
MgO 12.60% 0.55
Na2O 1.30% 0.04
TiO2 0.30% 0.01
Al2O3 6.50% 0.11
P2O5 0.20% -
SiO2 45.40% 1.34
Fe2O3 2.20% 0.02
LOI 17.20%n/a
Oxide Weight 146.63
Formula Weight 177.08

Notes

A California calcium, low swelling, colloidal type bentonite clay. It is prime for water impedance, asphalt coating applications, drilling mud and is also used in such products as paints, adhesives and cleaning compounds where absorption and body are needed. It is the most grit-free bentonite produced for commercial scale.

Physical Properties

Specific Gravity: 2.6
Apparent Density (lbs/cu. ft): 47 for 200 mesh, 60 for 50 mesh
Tapped Density (lbs/cu. ft): 73/83
Dry Brightness: 56 for 200 mesh, 51 for 50 mesh
pH: 9.7

Related Information

Links

Materials Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying.
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy