Hommel Frit 497

Description: Zinc magnesia borosilicate frit

Oxide Analysis Formula Tolerance
K2O 2.00% 0.09
Li2O 1.00% 0.14
MgO 4.00% 0.42
Na2O 2.00% 0.14
ZnO 4.00% 0.21
B2O3 25.00% 1.53
Al2O3 3.00% 0.12
SiO2 59.00% 4.17
Oxide Weight 424.73
Formula Weight 424.73

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 3.70
Frit Softening Point 1100F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy