Hommel Frit 446

Description: Leadless zinc high boron frit

Oxide Analysis Formula Tolerance
CaO 4.35% 0.18
Na2O 10.66% 0.40
ZnO 14.82% 0.42
B2O3 28.73% 0.96
SiO2 41.44% 1.60
Oxide Weight 231.73
Formula Weight 231.73

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3824
Materials Pemco Frit P-1733
Materials General Frit GF-100
Materials Fusion Frit FZ-16
The champion in our frit melt-off competitition. This frit showcases the amazing fluxing power of boron and zinc working together. It is 15.5% ZnO.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy