Hommel Frit 432

Oxide Analysis Formula Tolerance
K2O 6.63% 0.18
Na2O 3.07% 0.13
CaO 6.14% 0.28
MgO 1.59% 0.10
ZnO 10.00% 0.31
Al2O3 13.27% 0.33
B2O3 4.75% 0.17
SiO2 51.58% 2.19
ZrO2 2.97% 0.06
Oxide Weight 255.33
Formula Weight 255.33

Related Information

Links

Materials Fusion Frit FZ-164
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.9 x 10-6
Frit Melting Range (C) 1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy