Glasurfritten 37.031

Alternate Names: 37 031,37-031

Description: Bleifreie Kalzium-Borat-Fritte

Oxide Analysis Formula Tolerance
CaO 44.60% 0.69
BaO 55.40% 0.31
Oxide Weight 86.48
Formula Weight 86.48

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 85 x 10-7
Frit Softening Point 610C
Frit Melting Range (C) 700-1150C